Synthetic monocrystalline diamond wire dies

Physical Properties:

Hardness:Mohs hardness 10

Microhardness£º98654.9MPa£¨100060kg/mm2£©

Density:3470-3560kg/m3

Refractive index£º2.40-2.48

Thermal conductivity:136.16w/£¨m¡¤k£©

Dispersive power:0.044

The SMCD is suitable for the same applications as natural diamond dies.

Hole size range
from 0.020mm to 0.600mm

 